Eight dimensions side by side
| Dimension | VARTM resin infusion | OOA prepreg | Autoclave prepreg |
|---|---|---|---|
| Fiber volume fraction Vf | 45–55% | ~53–58% | 55–65%+ |
| Void content | 1–3%, operator dependent | <1–2% with good debulking | <1% |
| Pressure / temperature | ~1 bar (vacuum), ambient or oven post-cure | Vacuum only, oven 80–135 °C typical | 3–7 bar, 120–180 °C |
| Storage & out-life scrap | Dry fabric, infinite shelf life; resin mixed per shot | Freezer −18 °C, out-life tracked; expired material scrapped | Freezer −18 °C, out-life tracked; expired material scrapped |
| Tooling CapEx | Lowest: epoxy/glass tools, single-sided | Moderate: vacuum-tight, temperature-rated tools | Highest: pressure-rated, CTE-matched carbon or metal, egg-crate backed |
| Consumable waste per part | High: flow media, spiral, resin lines, catch pot | Moderate: breather, film, bag | Moderate: breather, film, bag, sealant |
| Labor skill | Infusion strategy and leak-free bagging | Prepreg layup, debulk discipline | Prepreg layup, autoclave scheduling and logging |
| Break-even guidance | One-offs and body panels where weight is secondary | Wings and panels when autoclave queue or cost is the bottleneck | Stressed aero, floors, structures, anything where stiffness-to-weight wins races |
Why the numbers differ
Consolidation pressure does two things: it squeezes excess resin out (higher Vf) and it collapses trapped air and volatiles (fewer voids). Infusion only has atmospheric pressure to work with, so the laminate carries more resin per ply and is heavier and less stiff for the same fiber. Autoclave prepreg starts with a controlled resin content (typically 38–42% by weight) and adds 3–7 bar on top of vacuum, which is why it is the default for dry carbon race parts.
Out-of-autoclave prepregs are formulated with partially impregnated "breathing" plies that let air escape under vacuum alone. With disciplined debulking they get close to autoclave quality on moderate thicknesses, and they remove the autoclave as a scheduling bottleneck.
Rule of thumb. Every 5 points of Vf is roughly 8–10% of laminate stiffness and a few percent of mass. On a splitter or wing that difference matters; on a dash panel it usually does not.
Decision framework by part class
| Part class | Typical parts | Recommended route | Why |
|---|---|---|---|
| Non-structural body panels | Dash, door cards, side skirts, covers | VARTM or OOA | Low load; tooling cost dominates small batches |
| Stressed aero | Splitter, undertray, wing elements, diffuser | Autoclave (OOA acceptable for club programs) | Stiffness-to-weight and fatigue under aero load |
| Hollow or closed sections | Wing mainplanes, struts, ducts with internal pressure | Autoclave or OOA with bladder | Internal pressure needs prepreg; infusion cannot consolidate it |
| Crash and safety structures | Survival cells, impact attenuators, fuel cell housings | Autoclave only, to the regulation | Homologation, traceability and void limits |
| High-temperature zones | Brake ducts, heat shields, engine bay | Autoclave or OOA with high-Tg resin | Resin Tg must clear heat soak with margin |
Compare all three routes on your part and batch size.
Run the process comparisonBatch size changes the answer
At quantity one, tooling is often 70–85% of the program, so the cheaper tool that VARTM allows can halve the bill. By 10–25 parts the recurring cost per part dominates; autoclave prepreg's lower scrap of rework and higher consistency usually make it the better buy, and the tool cost is spread thin. The estimator's process table shows exactly where that crossover lands for your area, geometry and stack.

What to put in the RFQ
- Part class and load: is it cosmetic, aero-loaded, or structural?
- Heat exposure, so the resin Tg can be chosen (see the prepreg & core guide).
- Quantity across the season, including spares.
- Any regulation that fixes the material or process (see motorsport composite regulations).